Hardness Conversion Calculator (HRC, HV, HB)

Convert a steel hardness between Rockwell C, Vickers and Brinell, with an estimate of the tensile strength.

How it works

Hardness scales measure different things (the depth of a dent, or the size of one), so there is no exact formula between them. Conversions come from tables of test results. This calculator interpolates between the rounded ASTM E140 values for non-austenitic steels, the same ones as in our hardness conversion chart.

between two table rows: value = lower + (x − xlower) ÷ (xupper − xlower) × (upper − lower)

tensile strength ≈ 3.45 × HB (MPa)

SymbolMeaningRange here
HRCRockwell C hardness (diamond cone, 150 kgf)20 to 60
HVVickers hardness (diamond pyramid)238 to 697
HBBrinell hardness (10 mm ball, 3,000 kgf)226 to 481
SuApproximate tensile strength of carbon and alloy steelfrom HB

The conversion applies to carbon and alloy steels in the heat-treated or as-rolled condition. It does not apply to austenitic stainless steel, cast iron, aluminum, brass or other metals, which have their own tables. Below HRC 20 the Rockwell C scale is not used: softer steels are measured in Rockwell B or Brinell. Above about HRC 50 Brinell values need a carbide ball and are not given here.

Related: Hardness Conversion Chart, Materials and Processes guide, Steel Grade Cross Reference.

Worked example

HRC 40 is a table row: HV 392 and HB 371, and the tensile strength is about 3.45 × 371 = 1,280 MPa (186 ksi).

HV 300 lies between the rows HV 266 (HRC 25, HB 253) and HV 302 (HRC 30, HB 286). The fraction is (300 − 266) ÷ (302 − 266) = 0.944, so HRC = 25 + 0.944 × 5 = 29.7 and HB = 253 + 0.944 × 33 = 284.

Things to know

A converted hardness is less certain than a measured one. Where a drawing or standard names a scale, test in that scale.

The tensile estimate (3.45 × HB in MPa, or about 500 × HB in psi) is good to roughly 10 percent for carbon and alloy steels and does not apply to other metals.

Thin parts, case-hardened layers and small features need a light-load test (Vickers, Knoop or superficial Rockwell); a heavy Brinell or Rockwell C test would punch through the hard layer.

Hardness is measured at the surface. A through-hardened part and a case-hardened part can show the same surface hardness with very different core strength.

Common questions

How do you convert HRC to HV?

Look it up in a conversion table and interpolate between rows. For example HRC 30 is about HV 302, HRC 40 about HV 392 and HRC 50 about HV 513 for steel.

How do you convert Brinell to Rockwell C?

By table: HB 286 is about HRC 30, HB 371 about HRC 40 and HB 481 about HRC 50. Below about HB 226 (HRC 20) Rockwell C is not used.

Is there a formula for hardness conversion?

Not an exact one. The scales use different indenters and loads, and the relationship depends on the material. Published formulas are curve fits to the same tables this calculator interpolates.

How do you estimate tensile strength from hardness?

For carbon and alloy steels, tensile strength in MPa is about 3.45 times the Brinell hardness (about 500 times HB in psi). HB 300 suggests roughly 1,035 MPa (150 ksi).

Sources

  • ASTM E140, Standard Hardness Conversion Tables for Metals (the values used here are rounded from the table for non-austenitic steels).
  • ISO 18265, Metallic materials: conversion of hardness values.

Last reviewed: November 11, 2026

Published by Nick Peterson, mechanical engineer.